Skip to main navigation Skip to search Skip to main content

Hierarchical petascale simulation framework for stress corrosion cracking

  • P. Vashishta
  • , R. K. Kalia
  • , A. Nakano
  • , E. Kaxiras
  • , A. Grama
  • , G. Lu
  • , S. Eidenbenz
  • , A. F. Voter
  • , R. Q. Hood
  • , J. A. Moriarty
  • , L. H. Yang

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution

1 Scopus citations
Original languageEnglish
Title of host publicationJournal of Physics: Conference Series
Volume78
Edition1
DOIs
StatePublished - Jul 1 2007
Externally publishedYes

Cite this