Abstract
The effect of sample thickness, strain rate, and temperature on the mechanical response of AdipreneL100 is presented. The compressive stress-strain response of Adiprene-L100 was found to depend on both the applied strain rate; 0.001 ≤ ε ≤ 7000 s-1, and the test temperature at high-rate; 77 ≤ Τ ≤ 298 K. Due to the slow, dispersive wave propagation in Adiprene-L100, thinner sample thicknesses are needed to assure uniform, uniaxial stress conditions within Hopkinson Bar samples; the optimal sample thickness being dependent on test temperature. Decreasing temperature from 298 to 77K at 3000 s-1 was found to increase the maximum flow stress in Adiprene-L 100 from 10 to ∼210 MPa.
| Original language | English |
|---|---|
| Pages (from-to) | C3-523-C3-528 |
| Number of pages | 1 |
| Journal | Journal De Physique. IV : JP |
| Volume | 7 |
| Issue number | 3 |
| State | Published - Aug 1 1997 |
Fingerprint
Dive into the research topics of 'Influence of temperature and strain rate on the mechanical behavior of adiprene L-100'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver