Initial stages of oxide growth on AM stainless steel exposed to a supercritical CO<inf>2</inf> environment

  • Michael A. Melia
  • , Samantha G. Rosenberg
  • , Paul G. Kotula
  • , Florent Bocher
  • , Rebecca F. Schaller

Research output: Contribution to journal › Article › peer-review

13 Scopus citations

Abstract

Wrought and additively manufactured (AM) 316 L stainless steel samples were exposed to a simulated Brayton cycle supercritical CO2 (sCO2) environment, at temperature of 450 °C and pressure of 76 bar in 99.999% CO2 for 2 weeks. The ground surfaces of wrought and AM 316 L specimens had average oxide thickness of 95 and 51 µm, respectively, composed primarily of Fe and Cr oxides. An as-printed AM 316 L sample was also exposed to the sCO2 environment and exhibited negligible oxidation during the 2-week exposure because of a thick Cr rich Mn silicate native oxide covering most of surface.
Original languageEnglish
JournalCorrosion Science
Volume201
DOIs
StatePublished - Jun 1 2022
Externally publishedYes

Fingerprint

Dive into the research topics of 'Initial stages of oxide growth on AM stainless steel exposed to a supercritical CO<inf>2</inf> environment'. Together they form a unique fingerprint.

Cite this