Molecular dynamic simulation of nanoindentation of cyclotrimethylenetrintramine (RDX) crystal

  • Yi Chun Chen
  • , Rajiv K. Kalia
  • , Aiichiro Nakano
  • , Ken Ichi Nomura
  • , Priya Vashishta

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Original languageEnglish
Title of host publicationMaterials Research Society Symposium Proceedings
Pages47-51
Number of pages5
Volume1021
StatePublished - Dec 1 2007