Skip to main navigation Skip to search Skip to main content

Nanoindentation of NiAl and Ni<inf>3</inf>Al crystals on (100), (110), and (111) surfaces: A molecular dynamics study

  • Richard Seymour
  • , Anne Hemeryck
  • , Ken Ichi Nomura
  • , Weiqiang Wang
  • , Rajiv K. Kalia
  • , Aiichiro Nakano
  • , Priya Vashishta

Research output: Contribution to journalArticlepeer-review

26 Scopus citations

Abstract

Molecular dynamics simulations were performed to study the nanoindentation of NiAl and Ni3Al crystals on three surfaces: (100), (110), and (111). The calculated load-displacement curves show discrete drops at certain indentation depths, indicating dislocation bursts during indentation. The hardness values for the two materials were found to depend significantly on the indented crystallographic plane: the (100) surface is the softest for NiAl and the hardest for Ni3Al. We also found distinctive deformation activities in the subsurface region in Ni3Al crystals, while dislocation loops propagate deep into the substrate in NiAl systems. © 2014 Author(s).
Original languageEnglish
JournalApplied Physics Letters
Volume104
Issue number14
DOIs
StatePublished - Apr 7 2014
Externally publishedYes

Fingerprint

Dive into the research topics of 'Nanoindentation of NiAl and Ni<inf>3</inf>Al crystals on (100), (110), and (111) surfaces: A molecular dynamics study'. Together they form a unique fingerprint.

Cite this